Operational Degradation of Spheroidal Graphite Cast Iron En Gjs Simo
dc.contributor.author | Skrbek Břetislav | cs |
dc.date.accessioned | 2018-09-25T12:10:36Z | |
dc.date.available | 2018-09-25T12:10:36Z | |
dc.date.issued | 2017 | cs |
dc.format.extent | 6 | cs |
dc.identifier.isbn | 978-80-01-06150-3 | cs |
dc.identifier.uri | https://dspace.tul.cz/handle/15240/30680 | |
dc.language.iso | cze | cs |
dc.publisher | ČVUT v Praze, Fakulta strojní a Výzkumný a zkušební ústav Plzeň s.r.o. | cs |
dc.publisher.city | Praha | cs |
dc.relation.ispartofseries | 0 | cs |
dc.subject | low-alloyed cast iron | cs |
dc.subject | Boundary exposition | cs |
dc.subject | Structure failure | cs |
dc.title | Operational Degradation of Spheroidal Graphite Cast Iron En Gjs Simo | en |
dc.title | Provozní degradace litin s kuličkovým grafitem typu EN GJS SiMo | cs |
local.citation.epage | 63-68 | cs |
local.citation.spage | 63-68 | cs |
local.identifier.publikace | 4130 |